PAVE

Guide

The four treatments

What each treatment is, when RxPave considers it, and what to plan for when it's viable.

This guide is also RxPave’s in-app help. Its tables are generated from the app’s own rules.

RxPave checks four treatments. This guide describes each one: what it is, when RxPave considers it, and what to plan for if it's viable. When more than one treatment is viable, weigh life-cycle cost, construction cost, expected life and the design and construction notes below. RxPave doesn't choose between viable treatments for you.

Which distresses rule each treatment out is in the scoring table.

Chip seal and cape seal

A chip seal (also called a bituminous surface treatment, or BST) is a sprayed asphalt emulsion covered with aggregate chips, rolled to embed them. It is a thin, waterproof wearing surface. A cape seal is a chip seal with a slurry seal placed over it, usually 4 to 10 days later, for a smoother surface.

  • When RxPave considers it: PCR 40 to 80.
  • What rules it out: high bleeding or flushing; medium or high rutting; high patching; and high alligator cracking.
  • Typical life: 7 to 10 years for a chip seal, 7 to 15 for a cape seal.
  • What it does: waterproofs the pavement, restores skid resistance, and seals small to moderate cracks and raveled surfaces. It adds no structural strength and doesn't correct rutting.

What RxPave will tell you

WhenRxPave says
Always, when chip seal is viableTraffic Levels. While appropriate for all traffic levels, chip seals tend to perform best on routes with at most 10,000 ADT (average daily traffic).
The segment has an intersection or a two-way left-turn laneTurning Movements. You indicated (or are uncertain of) the presence of an intersection or two-way left turn lane(s) in your segment. Compared to the rest of your segment, these areas may have different loading conditions and, consequently, pavement designs. If your roadway experiences significant turning movements, a chip or cape seal is not recommended for these areas. Instead, for these areas consider a 3/8-inch asphalt overlay at intersections of arterials and collectors, and at intersections subject to regular heavy-vehicle (e.g., buses, dump trucks) turning movements. Turning movements on an uncured surface may result in scuff marks.
Alligator cracking over less than 15% of the wheelpath areaPavement Distress (Alligator Cracking). You indicated alligator cracking over less than 15% of the wheelpath area. Repair and patch small localized areas before chip sealing; chip seals suit alligator cracks under 1/8 inch wide.
Transverse or longitudinal cracking is presentPavement Distress (Transverse and/or Longitudinal Cracking). You indicated the presence of transverse and/or longitudinal cracking. Cracks greater than 1/8 inch should be crack sealed and completely cured prior to chip sealing.
Bleeding or flushing is presentPavement Distress (Bleed/Flush). You indicated the presence of bleeding or flushing on your segment. You should repair any flushed areas on the surface before the chip seal application. Placing chip seals over existing flushed surfaces may result in flushing/bleeding reappearing on the new chip seal.
Moderate flushing in the wheelpaths, and a smooth surface is wantedAdditional Considerations. Consider a double chip seal in the wheelpaths, and a cape seal to provide smooth macro-texture.
Moderate flushing in the wheelpaths; a smooth surface is not neededAdditional Considerations. Consider a double chip seal in the wheelpaths.
A smooth surface is wanted for bikes, pedestrians or appearance; no wheelpath flushingAdditional Considerations. Consider a cape seal to provide smooth macro-texture.
You answered Unsure about wheelpath flushing or a smooth surfaceAdditional Considerations. You indicated uncertainty about wheelpath flushing or the need for a smooth macro-texture. If there is moderate flushing in the wheelpath, consider a double chip seal in the wheelpaths; if your design requires a smooth macro-texture, consider a cape seal.

Variations

  • Choke stone: smaller stone spread right after the chips. It locks into the voids, holds the chips while the binder cures, and gives a smoother texture.
  • Fog seal: a light coat of diluted emulsion over the finished chip seal. It helps hold the chips and improves the look.
  • Cape seal: the chip seal goes down without choke stone or fog seal, and a slurry seal (emulsified asphalt, water, fine aggregate and mineral filler) is spread over it once it has cured, after brushing.

Design and construction notes

  • For a chip seal, use choke stone and a fog seal. For about 5% more cost they reduce the risk of early failure and look better. WSDOT routinely uses choke stone and often a fog seal.
  • Use a polymer-modified emulsion to help hold the chips. WSDOT typically uses CRS-2P.
  • Repair flushed areas before chip sealing. A chip seal over a flushed surface can bleed.
  • Keep traffic off until the seal has cured, typically at least 24 hours. If traffic must use it, keep speeds under 25 mph to limit chip loss. Turning on an uncured surface scuffs it.
  • Use no more than 70 tons per lane-mile of ⅜-inch HMA leveling course under a chip seal.
  • Chip seals usually fail by flushing or by losing aggregate, and most failures happen in the first one or two years. One still in good condition after year two is likely to reach its expected life.

Thin hot mix asphalt (HMA) overlay

A thin layer of new hot mix asphalt, usually 1 to 2 inches, placed over the existing asphalt pavement, with or without milling first.

  • When RxPave considers it: PCR 30 to 65.
  • What rules it out: high bleeding or flushing; high rutting; high patching; and high alligator cracking.
  • Typical life: 10 to 20 years.
  • What it does: corrects surface defects, improves ride, skid resistance and drainage. It adds no structural strength.

What RxPave will tell you

WhenRxPave says
The segment has an intersection or a two-way left-turn laneTurning Movements. You indicated (or are uncertain of) the presence of an intersection or two-way left turn lane(s) in your segment. Consider using a 3/8-inch asphalt overlay at intersections of arterials and collectors, and at intersections subject to regular heavy-vehicle (e.g., buses, dump trucks) turning movements.
Geotextiles or other geosynthetics are presentGeosynthetics. You indicated the presence of geosynthetic materials, the use of which risks trapping moisture in the pavement. Overall, geosynthetics are not recommended as the risks generally outweigh potential benefits. Geosynthetics are intended to control reflective cracking propagating from the existing pavement to the overlay and may also act as a moisture barrier. However, geosynthetics are not effective in reducing reflection of thermal cracks, in areas of heavy rainfall, or in areas with significant freeze-thaw cycles.
A curb must be matchedCurb to Match. You have indicated the presence of a curb to match. RxPave recommends that you integrate this constraint in your resulting pavement design.
Chip seal and overlay score the same, or the curb reveal must be keptAdditional Considerations. Consider a 1-inch HMA overlay with a 9.5 mm or 4.75 mm NMAS mix.
You answered Unsure about keeping the curb reveal, and chip seal and overlay don't score the sameAdditional Considerations. You indicated uncertainty about keeping the curb reveal. If your resulting pavement must maintain curb reveal, consider a 1-inch HMA overlay with a 9.5 mm or 4.75 mm NMAS mix.

Variations

  • Milling: remove the surface to the depth of the overlay first. This removes surface defects above the mill depth and keeps curb height.
  • Mix design: a mix is specified by its PG binder grade (WSDOT's standard grades are PG 64-22 west of the Cascades and PG 64-28 east), its nominal maximum aggregate size (NMAS, typically ⅜ inch or ½ inch) and its gradation (dense-graded is recommended).
  • Geosynthetics are not recommended under a thin overlay: they can trap moisture, don't stop thermal cracks reflecting through, and don't work well with heavy rain or many freeze-thaw cycles.

Design and construction notes

  • Use a ⅜-inch mix. Low-traffic pavements benefit from its higher asphalt content, and it is easier to place and less prone to segregation. For a 1-inch overlay, consider a 4.75 mm mix. On a regular bus or truck route, consider a ½-inch mix.
  • Mill only if at least 2 to 3 inches of sound HMA will remain. Thinner remaining layers can break under the milling machine or heavy equipment.
  • Apply a tack coat to the existing or milled surface. It is a cheap way to prevent bond failure.
  • Make the overlay at least 3 times as thick as the NMAS, or it will be hard to compact.
  • Measure the finished density, preferably with cores or a nuclear gauge.
  • A thin overlay alone can't fix a very rough surface. Consider milling or a leveling course.

Full depth reclamation (FDR)

The existing pavement is pulverized in place to a set depth, mixed with a stabilizer, compacted and shaped, then surfaced with a chip seal or a thin HMA overlay.

  • When RxPave considers it: PCR 0 to 50.
  • What rules it out: any raveling; low bleeding or flushing; low rutting; and low or medium block, transverse or longitudinal cracking. So does any of the site conflicts below.
  • Typical life: 7 to 10 years with a chip seal surface, 10 to 20 with an overlay.
  • What it does: builds a new pavement structure from the old one. It is an alternative to reconstruction, or to repairs that would dig out more than about 20% of the area, and it corrects base failures, extensive alligator cracking, wide cracks, deep ruts, and profile and slope problems.

What rules it out on site

RxPave rules FDR out if the segment has any of:

  • geosynthetic materials
  • shallow utilities less than 1 ft from the surface
  • a treated base
  • concrete layers
  • a rigid (concrete) pavement
  • a composite pavement (asphalt over concrete)

A saturated subgrade or base is also a poor candidate, because the wet condition is likely to persist and cause future failure. RxPave doesn't ask about it, so check it yourself.

Variations

  • Stabilizer: usually cement, or foamed asphalt with an active filler (portland cement or lime), depending on the material being stabilized. Each has its own construction cautions.
  • Other in-place recycling: hot in-place recycling corrects minor surface defects; cold in-place recycling works within the existing asphalt layers only.

Design and construction notes

  • Take cores to find the subgrade's soil class, gradation, unconfined compressive strength and CBR. They decide the stabilizer and the reclamation depth. Have a pavement engineer set the stabilizer type and amount and the pavement design.
  • Too much stabilizer (more than about 5% cement) can crack the FDR layer, and the cracks reflect through the surface. Reduce the stabilizer rather than adding geosynthetics.
  • FDR can carry traffic for a while before it is surfaced. Heavy traffic may ravel it; a fog seal helps. Broom the surface before opening it.
  • Where it qualifies, FDR typically costs 30% to 60% less than reconstruction, because it reuses the existing material in place.

Full reconstruction

The existing pavement and base are removed and replaced with a new pavement structure.

  • When RxPave considers it: PCR 0 to 50.
  • What rules it out: any raveling; low bleeding or flushing; low rutting; and low or medium block, transverse or longitudinal cracking.
  • Typical life: 10 to 20 years for the surface; 40 years or more for the structure.
  • What it does: replaces the whole structure, with equal or better subbase, base and surface layers, so it addresses the most severe distresses.

FDR and reconstruction have the same PCR range and the same scores. What separates them is the site check: when FDR is ruled out on site, reconstruction is usually the answer.

What RxPave will tell you

WhenRxPave says
Existing subgrade CBR is below 8CBR Minimum. Before reconstruction, strengthen the subgrade, or remove and replace it, to reach a CBR of at least 10.

Variations

  • Interlocking concrete block pavement: precast concrete pavers on bedding sand, in place of the asphalt surface. A permeable version can form part of a drainage solution. Pavers can be lifted for work underneath and relaid. They suit speeds up to 45 mph; settlement is the main risk. RxPave doesn't score them separately: consider them wherever full reconstruction is viable.

Design and construction notes

  • Build at least 5 inches of HMA over at least 6 inches of crushed stone base. The 5 inches allow later mill-and-inlay work and make failure top-down rather than bottom-up.
  • Make the structure at least half the design frost depth, if nothing else is specified. Thickening the crushed base is the cheapest way there.
  • Compact the subgrade and base to at least 98% of modified Proctor density (ASTM D1557), and the HMA to at least 92%, measured with cores or a nuclear gauge. Pave the HMA in two lifts.
  • Use a ⅜-inch mix, or ½ inch on a regular bus or truck route.
  • Top-down cracking caught early can be corrected by milling and filling to at least the crack depth.

Relative cost

RxPave doesn't estimate cost. As a rough order, from the research: chip and cape seals cost least; FDR (plus its surfacing) and a thin overlay cost several times more; full reconstruction costs the most. For the research's Washington cost ranges, see Part 4 of the study in Research and references.