RxPave helps you choose a rehabilitation treatment for one segment of a low-volume road. It checks four treatments against what you tell it about the segment and reports which ones are viable, why the others are not, and what to watch for with each. Every rule below is published, so you can check any result by hand. The tables on this page are generated from the same data RxPave scores with.
The four treatments:
| Treatment | What it is | Typical life |
|---|---|---|
| Chip seal and cape seal | A sprayed asphalt emulsion covered with aggregate chips; a cape seal adds a slurry seal on top for a smoother surface | 7–10 years (chip), 7–15 years (cape) |
| Thin hot mix asphalt (HMA) overlay | A 1–2 inch asphalt wearing surface, with or without milling | 10–20 years |
| Full depth reclamation (FDR) | The existing pavement is pulverized and stabilized in place, then surfaced with a chip seal or overlay | 7–10 years with a chip seal, 10–20 with an overlay |
| Full reconstruction | The pavement structure is removed and replaced | Surface 10–20 years; structure 40+ years |
The method comes from research by the University of Washington for the Washington State Transportation Improvement Board (TIB): Recommended SCPP Treatment Scoping Process (2015). RxPave applies its scoring table and flowcharts exactly.
The short version
A treatment is viable when it passes all four checks:
- Condition: the segment's Pavement Condition Rating (PCR) is inside the treatment's range.
- Distresses: nothing in your distress survey rules the treatment out.
- Score: its distress score is the top score, or within 1 point of it.
- Site: nothing about the existing road rules it out (this check applies to FDR).
Then RxPave adds considerations: advice specific to each viable treatment, based on your answers. Considerations never rule a treatment out.
Check 1 — Pavement condition (PCR)
Each treatment suits a range of condition. RxPave compares your last PCR reading (0–100, higher is better) with these ranges, including both ends:
| Treatment | PCR range |
|---|---|
| Chip seal and cape seal | 40 – 80 |
| Thin HMA overlay | 30 – 65 |
| Full depth reclamation | 0 – 50 |
| Full reconstruction | 0 – 50 |
What this means in practice:
- Above 80, no treatment is in range. The road is in good enough condition that rehabilitation is probably not needed yet; RxPave says so rather than recommending anything.
- Below 30, only FDR and reconstruction are in range.
- FDR and reconstruction have the same range and, as you'll see below, the same scores. What separates them is the site check (Check 4).
If your PCR reading is more than 4 years old, RxPave still uses it but warns you, because pavement condition declines with age.
Check 2 — Distresses
You rate eight distresses as None, Low, Medium or High. For each one, every treatment gets:
- 2 points: recommended, usually the best treatment for this distress.
- 1 point: conditional, it can work, with some risk or extra cost.
- Ruled out: the treatment is inappropriate for this distress (too risky or too expensive). A treatment ruled out by any one distress is not viable.
- 0 points: the distress isn't present.
The scoring table
L = Low, M = Medium, H = High. ✕ = ruled out.
| Distress | Chip / cape seal L · M · H | Thin HMA overlay L · M · H | Full depth reclamation L · M · H | Full reconstruction L · M · H |
|---|---|---|---|---|
| Raveling | 2 · 2 · 1 | 1 · 1 · 2 | ✕ · ✕ · ✕ | ✕ · ✕ · ✕ |
| Bleed/Flush | 1 · 1 · ✕ | 1 · 1 · ✕ | ✕ · 1 · 2 | ✕ · 1 · 2 |
| Rutting | 1 · ✕ · ✕ | 2 · 1 · ✕ | ✕ · 2 · 2 | ✕ · 2 · 2 |
| Patching | 1 · 1 · ✕ | 1 · 1 · ✕ | 1 · 1 · 2 | 1 · 1 · 2 |
| Alligator Cracking | 2 · 1 · ✕ | 2 · 2 · ✕ | 1 · 1 · 2 | 1 · 1 · 2 |
| Block Cracking | 2 · 1 · 1 | 1 · 2 · 1 | ✕ · ✕ · 1 | ✕ · ✕ · 1 |
| Transverse Cracking | 2 · 1 · 1 | 1 · 2 · 1 | ✕ · ✕ · 1 | ✕ · ✕ · 1 |
| Longitudinal Cracking | 2 · 1 · 1 | 1 · 1 · 2 | ✕ · ✕ · 1 | ✕ · ✕ · 1 |
Some patterns worth knowing:
- Any raveling rules out FDR and reconstruction. Raveling is a surface problem; rebuilding the structure is the wrong tool.
- Low bleeding or rutting rules out FDR and reconstruction, while medium or high bleeding or rutting scores for them. Minor surface distress doesn't justify rebuilding; severe distress does.
- High bleeding, high patching, high alligator cracking and medium-or-high rutting rule out chip seals; the same list, except medium rutting, rules out overlays. These point to problems a surface treatment can't fix.
Severity definitions
| Distress | Low | Medium | High |
|---|---|---|---|
| Raveling | Patchy areas, usually in wheelpaths | Majority of wheelpaths affected | Most of the lane affected |
| Bleed/Flush | Patchy areas, usually in wheelpaths | Majority of wheelpaths affected | Most of the lane affected |
| Rutting | Rut depth ≤ ¼ in | ¼ to ¾ in | > ¾ in |
| Patching | ≤ 5% of surface area | 6% to 25% | > 25% |
| Alligator Cracking | Hairline | Spalling | Spalling and pumping |
| Block Cracking | Cracks ≤ ¼ in wide | Cracks over ¼ in, no spalling | Cracks over ¼ in with spalling |
| Transverse Cracking | 1 to 4 cracks per 100 ft | 5 to 9 per 100 ft | 10 or more per 100 ft |
| Longitudinal Cracking | Total crack length 1% to 99% of the segment length | 100% to 199% | 200% or more |
Judge raveling and bleeding by the area affected, not by how much aggregate is lost or how much binder shows. Measure rut depth from the deepest point to the normal pavement surface, not to the raised lip beside the rut.
Before you survey: if there are isolated areas of base failure (severe alligator cracking or base rutting) covering less than 20% of the pavement, the research recommends leaving them out of the survey and repairing them separately: dig out to the depth of the failing base and replace with material of CBR 10 or more. If they cover more than 20%, FDR or reconstruction of the whole segment is likely cheaper.
Check 3 — Score
RxPave adds up each treatment's points across all eight distresses. A treatment passes this check if its total is the highest of the treatments still in the running (inside their PCR range and not ruled out) or within 1 point of it. More than one treatment can pass, and often does.
Check 4 — Site conflicts (FDR)
FDR pulverizes the existing pavement in place, so some things under or in the road make it a poor choice. RxPave rules FDR out if you tell it the segment has any of:
- geosynthetic materials
- shallow utilities less than 1 ft from the surface
- a treated base
- concrete layers
- a rigid (concrete) pavement
- a composite pavement (asphalt over concrete)
Reconstruction remains available in these cases; that is usually what separates the two.
Considerations
Considerations are advice for a viable treatment. They never change which treatments are viable. The advice is shown in RxPave's own words.
Chip seal and cape seal
| When | RxPave says |
|---|---|
| Always, when chip seal is viable | Traffic Levels. While appropriate for all traffic levels, chip seals tend to perform best on routes with at most 10,000 ADT (average daily traffic). |
| The segment has an intersection or a two-way left-turn lane | Turning Movements. You indicated (or are uncertain of) the presence of an intersection or two-way left turn lane(s) in your segment. Compared to the rest of your segment, these areas may have different loading conditions and, consequently, pavement designs. If your roadway experiences significant turning movements, a chip or cape seal is not recommended for these areas. Instead, for these areas consider a 3/8-inch asphalt overlay at intersections of arterials and collectors, and at intersections subject to regular heavy-vehicle (e.g., buses, dump trucks) turning movements. Turning movements on an uncured surface may result in scuff marks. |
| Alligator cracking over less than 15% of the wheelpath area | Pavement Distress (Alligator Cracking). You indicated alligator cracking over less than 15% of the wheelpath area. Repair and patch small localized areas before chip sealing; chip seals suit alligator cracks under 1/8 inch wide. |
| Transverse or longitudinal cracking is present | Pavement Distress (Transverse and/or Longitudinal Cracking). You indicated the presence of transverse and/or longitudinal cracking. Cracks greater than 1/8 inch should be crack sealed and completely cured prior to chip sealing. |
| Bleeding or flushing is present | Pavement Distress (Bleed/Flush). You indicated the presence of bleeding or flushing on your segment. You should repair any flushed areas on the surface before the chip seal application. Placing chip seals over existing flushed surfaces may result in flushing/bleeding reappearing on the new chip seal. |
| Moderate flushing in the wheelpaths, and a smooth surface is wanted | Additional Considerations. Consider a double chip seal in the wheelpaths, and a cape seal to provide smooth macro-texture. |
| Moderate flushing in the wheelpaths; a smooth surface is not needed | Additional Considerations. Consider a double chip seal in the wheelpaths. |
| A smooth surface is wanted for bikes, pedestrians or appearance; no wheelpath flushing | Additional Considerations. Consider a cape seal to provide smooth macro-texture. |
| You answered Unsure about wheelpath flushing or a smooth surface | Additional Considerations. You indicated uncertainty about wheelpath flushing or the need for a smooth macro-texture. If there is moderate flushing in the wheelpath, consider a double chip seal in the wheelpaths; if your design requires a smooth macro-texture, consider a cape seal. |
Thin HMA overlay
| When | RxPave says |
|---|---|
| The segment has an intersection or a two-way left-turn lane | Turning Movements. You indicated (or are uncertain of) the presence of an intersection or two-way left turn lane(s) in your segment. Consider using a 3/8-inch asphalt overlay at intersections of arterials and collectors, and at intersections subject to regular heavy-vehicle (e.g., buses, dump trucks) turning movements. |
| Geotextiles or other geosynthetics are present | Geosynthetics. You indicated the presence of geosynthetic materials, the use of which risks trapping moisture in the pavement. Overall, geosynthetics are not recommended as the risks generally outweigh potential benefits. Geosynthetics are intended to control reflective cracking propagating from the existing pavement to the overlay and may also act as a moisture barrier. However, geosynthetics are not effective in reducing reflection of thermal cracks, in areas of heavy rainfall, or in areas with significant freeze-thaw cycles. |
| A curb must be matched | Curb to Match. You have indicated the presence of a curb to match. RxPave recommends that you integrate this constraint in your resulting pavement design. |
| Chip seal and overlay score the same, or the curb reveal must be kept | Additional Considerations. Consider a 1-inch HMA overlay with a 9.5 mm or 4.75 mm NMAS mix. |
| You answered Unsure about keeping the curb reveal, and chip seal and overlay don't score the same | Additional Considerations. You indicated uncertainty about keeping the curb reveal. If your resulting pavement must maintain curb reveal, consider a 1-inch HMA overlay with a 9.5 mm or 4.75 mm NMAS mix. |
Full reconstruction
| When | RxPave says |
|---|---|
| Existing subgrade CBR is below 8 | CBR Minimum. Before reconstruction, strengthen the subgrade, or remove and replace it, to reach a CBR of at least 10. |
For the whole segment
| When | Shown in | RxPave says |
|---|---|---|
| The PCR reading is more than 4 years old | Report | PCR Collection Date. The PCR reading is over 4 years old and may no longer accurately represent current conditions. |
| Parking lanes, shoulders or bike lanes are present | Report | Differing Pavement Designs. You have indicated the presence of parking lanes, shoulders, or bicycle lanes. These pavement areas may experience different traffic loading conditions than the mainline and consequently may feature a different pavement design. Further investigation may be needed to determine whether or not these areas must also be rehabilitated or preserved. |
| The last treatment is unknown | Form and report | Last Treatment Unknown. The type and age of the last treatment are potential indicators of an underperforming treatment in RxPave. For example, chip and cape seals have expected lives of 7–10 years, HMA overlays 10–20 years, and reconstructed pavements have structural lives of at least 40 years. |
| The last treatment was a chip or cape seal less than 7 years ago | Form and report | Expected Life of Last Treatment Underperforming. You indicated that the last treatment on the segment was a chip seal (or FDR with a chip seal) performed less than 7 years ago. As the expected life of a chip seal is 7–10 years, your pavement may be underperforming. |
| The last treatment was an overlay less than 10 years ago | Form and report | Expected Life of Last Treatment Underperforming. You indicated that the last treatment on the segment was an HMA overlay (or FDR with an HMA overlay) performed less than 10 years ago. As the expected life of an HMA overlay is 10–20 years, your pavement may be underperforming. |
| The last treatment was a reconstruction less than 10 years ago | Form and report | Expected Life of Last Treatment Underperforming. You indicated that the last treatment on the segment was a full reconstruction completed less than 10 years ago. As the expected life of a fully reconstructed surface is 10–20 years, your pavement may be underperforming. |
| The PCR reading is from before the year of the last treatment | Form and report | PCR Older Than Last Treatment. The last PCR reading is not newer than the most recently reported rehabilitation activity. Further investigation may be warranted as this suggests that your PCR rating is outdated or inconsistent with actual current pavement conditions. |
| Rigid or composite pavement, but concrete layers are not answered Yes | Form and report | Pavement Type and Concrete Layers. You indicated that the existing pavement type is rigid or composite, but did not specify the presence of concrete layers. Please review this information for accuracy. |
When you answer "Unsure"
"Unsure" is treated the safe way: as Yes for anything that could rule a treatment out or prompt a warning. For example, if you're unsure whether the road has geotextiles, RxPave rules out FDR and tells you why, so you know what to find out.
The additional factors on the last step are optional. Leave one unanswered and RxPave still scores the segment; the advice that depends on it doesn't appear.
Worked examples
These tables are produced by running RxPave on each example when this page is built.
Example 1 — surface cracking, fair condition
PCR 45. Low alligator cracking over 10% of the wheelpath, medium transverse cracking, low block cracking. No site conflicts.
| Alligator Cracking L | Transverse Cracking M | Block Cracking L | Total | PCR 45 in range? | Viable? | |
|---|---|---|---|---|---|---|
| Chip / cape seal | 2 | 1 | 2 | 5 | yes (40–80) | Yes |
| Thin HMA overlay | 2 | 2 | 1 | 5 | yes (30–65) | Yes |
| Full depth reclamation | 1 | ✕ | ✕ | 1 | yes (0–50) | No — ruled out by block cracking and transverse cracking |
| Full reconstruction | 1 | ✕ | ✕ | 1 | yes (0–50) | No — ruled out by block cracking and transverse cracking |
Considerations shown: Chip / cape seal: Traffic Levels, Pavement Distress (Alligator Cracking), Pavement Distress (Transverse and/or Longitudinal Cracking); Thin HMA overlay: Additional Considerations.
Example 2 — structural failure, poor condition
PCR 25. High alligator cracking, high rutting, medium patching.
| Alligator Cracking H | Rutting H | Patching M | Total | PCR 25 in range? | Viable? | |
|---|---|---|---|---|---|---|
| Chip / cape seal | ✕ | ✕ | 1 | 1 | no | No — PCR outside 40–80; ruled out by rutting and alligator cracking |
| Thin HMA overlay | ✕ | ✕ | 1 | 1 | no | No — PCR outside 30–65; ruled out by rutting and alligator cracking |
| Full depth reclamation | 2 | 2 | 1 | 5 | yes (0–50) | Yes |
| Full reconstruction | 2 | 2 | 1 | 5 | yes (0–50) | Yes |
Same road, but the base is cement-treated: FDR is ruled out by the site check, and reconstruction is the only viable treatment.
| Alligator Cracking H | Rutting H | Patching M | Total | PCR 25 in range? | Viable? | |
|---|---|---|---|---|---|---|
| Chip / cape seal | ✕ | ✕ | 1 | 1 | no | No — PCR outside 40–80; ruled out by rutting and alligator cracking |
| Thin HMA overlay | ✕ | ✕ | 1 | 1 | no | No — PCR outside 30–65; ruled out by rutting and alligator cracking |
| Full depth reclamation | 2 | 2 | 1 | 5 | yes (0–50) | No — ruled out by the site check |
| Full reconstruction | 2 | 2 | 1 | 5 | yes (0–50) | Yes |
Example 3 — good condition
PCR 85: no treatment's range reaches 85, so RxPave recommends none and explains that the pavement may not need rehabilitation yet.
| Transverse Cracking L | Block Cracking L | Total | PCR 85 in range? | Viable? | |
|---|---|---|---|---|---|
| Chip / cape seal | 2 | 2 | 4 | no | No — PCR outside 40–80 |
| Thin HMA overlay | 1 | 1 | 2 | no | No — PCR outside 30–65 |
| Full depth reclamation | ✕ | ✕ | 0 | no | No — PCR outside 0–50; ruled out by block cracking and transverse cracking |
| Full reconstruction | ✕ | ✕ | 0 | no | No — PCR outside 0–50; ruled out by block cracking and transverse cracking |
RxPave says: The PCR of 85 is above every treatment's range (the highest is 80). The pavement's condition may be high enough that rehabilitation is unnecessary for now.
Example 4 — chip seal with flushing
PCR 60. Medium raveling, low bleeding, high longitudinal cracking; moderate wheelpath flushing; a smooth surface is wanted.
| Raveling M | Bleed/Flush L | Longitudinal Cracking H | Total | PCR 60 in range? | Viable? | |
|---|---|---|---|---|---|---|
| Chip / cape seal | 2 | 1 | 1 | 4 | yes (40–80) | Yes |
| Thin HMA overlay | 1 | 1 | 2 | 4 | yes (30–65) | Yes |
| Full depth reclamation | ✕ | ✕ | 1 | 1 | no | No — PCR outside 0–50; ruled out by raveling and bleeding or flushing |
| Full reconstruction | ✕ | ✕ | 1 | 1 | no | No — PCR outside 0–50; ruled out by raveling and bleeding or flushing |
Considerations shown: Chip / cape seal: Traffic Levels, Pavement Distress (Transverse and/or Longitudinal Cracking), Pavement Distress (Bleed/Flush), Additional Considerations; Thin HMA overlay: Additional Considerations.
What RxPave doesn't do
RxPave scopes; it doesn't design. It doesn't size layers, estimate cost or life-cycle cost, or choose between viable treatments for you. When more than one treatment is viable, the research suggests weighing life-cycle cost, construction cost, expected life and project-specific design and construction factors. When the project moves on to design, construction inspection and daily reports, see who makes RxPave.
Sources
- Muench, S.T. and Yamaura, J. (2015). *Assessment and Update of TIB Urban Program and Small City Preservation Program, Part 4: Recommended SCPP Treatment Scoping Process.* University of Washington for the Washington State Transportation Improvement Board. Scoring table: Figure 3 (p.7); PCR ranges: Figure 2 (p.6); flowcharts: Figure 1 (p.4–5); treatment guidance: p.10–17.
- Part 3 of the same study (FDR State of the Practice) on why geotextiles and shallow utilities favor reconstruction over FDR.
Notes on the published research. Two flowchart conditions in Figure 1 are printed backwards ("80 ≤ PCR ≤ 40", "65 ≤ PCR ≤ 30"); RxPave uses the ranges from Figure 2. In the reconstruction flowchart, the arrow from "Is existing subgrade CBR < 8?" is labeled the wrong way round; RxPave follows the evident intent: strengthen the subgrade when CBR is below 8.